PBT - Non-Reinforced |
|
|
|
|
|
PBT, non-reinforced, extrusion, injection molding, improved flowability, suitable for food-contact |
Applications: |
|
Nonwovens, meltblown, spunbond, multifilaments, coatings |
|
|
|
|
|
|
PBT, non-reinforced, injection molding, improved flowability, improved impact strength |
|
|
|
|
|
|
PBT, non-reinforced, extrusion, base resin, improved flowability, suitable for food-contact
|
|
|
|
|
|
|
PBT, non-reinforced, injection molding, extrusion, improved flowability, suitable for food-contact
|
Applications: |
|
Filtration media from nonwoven, meltblown or spunbond; multifilaments, coatings |
|
|
|
|
|
|
PBT, non-reinforced, injection molding, improved flowability
|
|
|
|
|
|
PBT - glass fiber |
|
|
|
|
|
PBT, 10% glass fibers, injection molding, improved flowability, improved impact strength, improved electrical tracking resistance (CTI600) |
|
|
|
|
|
|
PBT, 10% glass fibers, injection molding, improved flowability, improved impact strength |
Applications: |
|
lamp socket |
|
|
|
|
|
|
PBT, 16% glass fibers, injection molding, improved flowability, improved impact strength, improved electrical tracking resistance (CTI600) |
|
|
|
|
|
|
PBT, 16% glass fibers, injection molding, improved flowability, improved impact strength |
|
|
|
|
|
|
PBT, 20% glass fibers, injection molding, improved flowability, improved impact strength |
Applications: |
|
lamp socket |
|
|
|
|
|
|
PBT, 30% glass fibers, injection molding, improved flowability, hydrolysis stabilized |
|
|
|
|
|
|
PBT, 30% glass fibers, injection molding, improved flowability, hydrolysis stabilized, improved electrical tracking resistance (CTI600) |
|
|
|
|
|
|
PBT, 30% glass fibers, injection molding, hydrolysis stabilized, improved flowability |
|
|
|
|
|
|
PBT, 30% glass fibers, injection molding, improved flowability, improved electrical tracking resistance (CTI600) |
|
|
|
|
|
|
PBT, 30% glass fibers, injection molding, improved flowability |
Applications: |
|
lamp socket |
|
|
|
|
|
|
PBT, 30% glass fibers, injection molding, improved flowability, hydrolysis stabilized |
|
|
|
|
|
|
PBT, 30% glass fibers, injection molding, hydrolysis stabilized, improved flowability |
|
|
|
|
|
PBT - glass beads |
|
|
|
|
|
PBT, 20% micro glass beads, injection molding, improved flowability, improved impact strength, low tendency to warp
|
|
|
|
|
|
|
PBT, 20% micro glass beads, injection molding, improved flowability, improved surface finish, improved electrical conductivity |
|
|
|
|
|
PBT+PC - glass fiber |
|
|
|
|
|
PBT+PC, 30% glass fibers, injection molding, improved flowability, low tendency to warp, improved surface finish
|
|
|
|
|
|
PBT+PET - glass fiber |
|
|
|
|
|
PBT+PET, 55% glass fibers, injection molding, improved flowability, low tendency to warp, increased temperature peak load, increased strength and increased modulus |
|
|
|
|
|
PET+PBT - glass fiber/mineral |
|
|
|
|
|
PET+PBT, 40% glass fibers/mineral, injection molding, improved flowability, high thermal dimension stability
|
|
|
|
|
|