PA6 - Non-Reinforced |
 |
 |
 |
 |
|
PA 6, non-reinforced, injection molding, improved impact strength |
Applications: |
|
Side window crank, cable clips, safty belt covers, wall-pegs, dowels, tool-handles |
|
|
 |
 |
 |
|
PA 6, non-reinforced, injection molding, improved impact strength
|
Applications: |
|
automotive bumber-parts, tool-grips, bike-fenders, ski-shoe parts, suitcase-rollers |
|
|
 |
 |
 |
|
PA 6, non-reinforced, injection molding, improved impact strength, heat-aging stabilized |
Applications: |
|
applicable for barrier layers in coextrusion blow molded containers for e.g. agrochemicals |
|
|
 |
 |
 |
|
PA 6, non-reinforced, blow molding, improved impact strength, heat-aging stabilized.
For the use in tank systems and pressure vessels please notice safety-related technical information within the High Performance Materials TechCenter under www.durethan-tank-systems.lanxess.com . |
|
|
 |
 |
 |
|
PA 6, non-reinforced, blow molding, improved impact strength, heat-aging stabilized.
For the use in tank systems and pressure vessels please notice safety-related technical information within the High Performance Materials TechCenter under www.durethan-tank-systems.lanxess.com . |
|
|
 |
 |
 |
|
PA 6, non-reinforced, blow molding, improved impact strength, heat-aging stabilized.
For the use in tank systems and pressure vessels please notice safety-related technical information within the High Performance Materials TechCenter under www.durethan-tank-systems.lanxess.com. |
|
|
 |
 |
 |
PA6 - glass fiber |
 |
 |
 |
 |
|
PA 6, 15% glass fibers, injection molding, improved impact strength
|
|
|
 |
 |
 |
Durethan BKV115H2.0 000000 |
|
|
PA 6, 15% glass fibers, injection molding, improved impact strength, heat-aging stabilized
|
|
|
 |
 |
 |
Durethan BKV115H3.0 000000 |
|
|
PA 6, 15% glass fibers, injection molding, improved impact strength, heat-aging stabilized
|
|
|
 |
 |
 |
|
PA 6, 30% glass fibers, injection molding, improved impact strength
|
|
|
 |
 |
 |
|
PA 6, 30% glass fibers, injection molding, improved impact strength |
|
|
 |
 |
 |
Durethan BKV130GIT 900116 |
|
|
PA 6, 30% glass fibers, injection molding, improved impact strength, GIT/WIT |
|
|
 |
 |
 |
Durethan BKV130H2.0 901510 |
|
|
PA 6, 30% glass fibers, injection molding, improved impact strength, heat-aging stabilized |
|
|
 |
 |
 |
|
PA 6, 30% glass fibers, injection molding, improved impact strength, improved flowability |
|
|
 |
 |
 |
Durethan BKV130H3.0 000000 DUS008 |
|
|
PA 6, 30% glass fibers, injection molding, improved impact strength, heat-aging stabilized |
|
|
 |
 |
 |
|
PA 6, 30% glass fibers, injection molding, improved impact strength, improved fatigue behavior |
|
|
 |
 |
 |
|
PA 6, 30% glass fibers, injection molding, improved impact strength, weather stabilized |
|
|
 |
 |
 |
|
PA 6, 40% glass fibers, injection molding, improved impact strength |
|
|
 |
 |
 |
Durethan BKV140H2.0 900051 |
|
|
PA 6, 40% glass fibers, injection molding, improved impact strength, heat-aging stabilized |
|
|
 |
 |
 |
|
PA 6, 20% glass fibers, injection molding, improved impact strength, heat-aging stabilized |
|
|
 |
 |
 |
|
PA 6, 30% glass fibers, injection molding, improved impact strength |
|
|
 |
 |
 |
Durethan BKV230H2.0 901510 |
|
|
PA 6, 30% glass fibers, injection molding, improved impact strength, heat-aging stabilized
|
|
|
 |
 |
 |
|
PA 6, 35% glass fibers, injection molding, improved impact strength, heat-aging stabilized |
|
|
 |
 |
 |
|
PA 6, 40% glass fibers, injection molding, improved impact strength, heat-aging stabilized |
|
|
 |
 |
 |
|
PA 6, 30% glass fibers, injection molding, improved weldability, heat-aging stabilized
|
|
|
 |
 |
 |
|
PA 6, 15% glass fibers, injection molding, improved impact strength |
|
|
 |
 |
 |
|
PA 6, 15% glass fibers, blow molding, improved impact strength, heat-aging stabilized
|
Applications: |
|
Automotive-sector: technical extruded and blow molded articles (hollow parts, air ducts), extruded sheets for thermoforming applications |
|
|
 |
 |
 |
|
PA 6, 20% glass fibers, blow molding, heat-aging stabilized |
|
|
 |
 |
 |
|
PA 6, 15% glass fibers, blow molding, improved impact strength, heat-aging stabilized
|
|
|
 |
 |
 |
|
PA 6, 25% glass fibers, blow molding, improved impact strength, heat-aging stabilized
|
|
|
 |
 |
 |
PA6-Copolymer - Non-Reinforced |
 |
 |
 |
 |
|
PA 6-Copolymer, non-reinforced, blow molding, heat-aging stabilized, improved impact strength, improved heat-aging stability.
For the use in tank systems and pressure vessels please notice safety-related technical information within the High Performance Materials TechCenter under www.durethan-tank-systems.lanxess.com . |
|
|
 |
 |
 |
PA6-Copolymer - glass fiber |
 |
 |
 |
 |
|
PA 6-Copolymer, 15% glass fibers, injection molding, improved impact strength, heat-aging stabilized
|
|
|
 |
 |
 |
|
PA 6-Copolymer, 30% glass fibers, injection molding, improved impact strength
|
Applications: |
|
Automotive seats and back rests, office chair-legs, seat-pans, full-plastic shopping-car |
|
|
 |
 |
 |
|
PA 6-Copolymer, 30% glass fibers, injection molding, improved impact strength
|
|
|
 |
 |
 |
|
PA 6-Copolymer, 30% glass fibers, injection molding, improved impact strength, GIT/WIT
|
Applications: |
|
Chain-saw handles, office chair armrests, office chair back rest |
|
|
 |
 |
 |
|
PA 6-Copolymer, 30% glass fibers, injection molding, improved impact strength, heat-aging stabilized
|
|
|
 |
 |
 |
|
PA 6-Copolymer, 30% glass fibers, injection molding, improved impact strength, heat-aging stabilized
|
|
|
 |
 |
 |
|
PA 6-Copolymer, 35% glass fibers, injection molding, improved impact strength
|
|
|
 |
 |
 |
|
PA 6-Copolymer, 40% glass fibers, injection molding, improved impact strength
|
|
|
 |
 |
 |
|
PA 6-Copolymer, 40% glass fibers, injection molding, improved impact strength, heat-aging stabilized
|
|
|
 |
 |
 |
|
PA 6-Copolymer, 15% glass fibers, injection molding, improved impact strength
|
Applications: |
|
Automotive sector: indoor window frame |
|
|
 |
 |
 |
|
PA 6-Copolymer, 15% glass fibers, injection molding, improved impact strength, heat-aging stabilized
|
Applications: |
|
Automotive sector: indoor window frame |
|
|
 |
 |
 |
|
PA 6-Copolymer, 15% glass fibers, injection molding, improved impact strength, heat-aging stabilized
|
|
|
 |
 |
 |
|
PA 6-Copolymer, 15% glass fibers, injection molding, improved impact strength, weather stabilized
|
|
|
 |
 |
 |
|
PA 6-Copolymer, 30% glass fibers, injection molding, improved impact strength, heat-aging stabilized
|
|
|
 |
 |
 |
|
PA 6-Copolymer, 30% glass fibers, injection molding, improved impact strength, heat-aging stabilized |
|
|
 |
 |
 |
|
PA 6-Copolymer, 30% glass fibers, injection molding, improved impact strength, weather stabilized
|
|
|
 |
 |
 |
|
PA 6-Copolymer, 30% glass fibers, injection molding, improved impact strength
|
|
|
 |
 |
 |
|
PA 6-Copolymer, 40% glass fibers, injection molding, improved impact strength |
|
|
 |
 |
 |
PA66 - Non-Reinforced |
 |
 |
 |
 |
|
PA 66, non-reinforced, injection molding, heat-aging stabilized, improved impact strength
|
|
|
 |
 |
 |
|
PA 66, non-reinforced, injection molding, improved impact strength, heat-aging stabilized
|
|
|
 |
 |
 |
Durethan DP2325H3.0 000000 |
|
|
PA 66, non-reinforced, injection molding, improved flowability, improved impact strength, heat-aging stabilized
|
|
|
 |
 |
 |
PA66 - glass fiber |
 |
 |
 |
 |
|
PA 66, 30% glass fibers, injection molding, improved impact strength, heat-aging stabilized
|
|
|
 |
 |
 |
|
PA 66, 15% glass fibers, blow molding, improved impact strength, heat-aging stabilized |
|
|
 |
 |
 |
|
PA 66, 20% glass fibers, blow molding, improved impact strength, heat-aging stabilized |
|
|
 |
 |
 |
|
PA 66, 20% glass fibers, blow molding, high temperature stabilized, improved impact strength |
|
|
 |
 |
 |
PA66 - mineral |
 |
 |
 |
 |
|
PA 66, 30% mineral, injection molding, improved impact strength, heat-aging stabilized, low tendency to warp |
|
|
 |
 |
 |
PA6I - glass fiber |
 |
 |
 |
 |
|